Me and my friend got a visitor from Germany,Axel Schnarrenberger, one of the big guys from Menzerna GMBH. Axel spent two days with us and tried to teach us some things about Menzerna, both practical and theoretical :graduation: Do I have to say it was great and very interesting?! Anyway, here are the pictures
Interested to know some of the highlights you gain from his visit. Most curious about polish and pad matching and advise on how far to work in some of the more popular Menzerna products like SIP. Also, any discussion about their new polymer sealant?
The sealant is a Menzerna USA product and Menzerna Germany has nothing to do with it. Interested as well what was learned.
Actualy, we never touched SIP :shead: products used: Fast gloss (S500), Power Finish (PO203) and super finish (PO106). Pads used: Menzerna wool, white (compouding) and white fine polishing/finishing. Good combinations: S500 and white compounding pad, P203 and PO106 with white fine pad and PO203 with wool. Worked ace! +1. But I got a lab coat instead =D
It sounds great Marcus !! Congratulations :worship2: I have to found how to clean the pads after using S500, because the abrassives stay inside of the pad, chech this: This is after just 1 panel. Cheers Marcus.
Thanks for the heads up, Mario, I have not noticed that. I will only use S500 with some pads and not mix them with other polishes.
How are you guys finding S500 compared to S100. More lubrication? It seems to have even more cut as well. How does it finish down? Sorry for all the questions.